Corrosion processes at the GGG40 steel–bentonite interface
Andrés G. Muñoz
CORRESPONDING AUTHOR
Repository Research, Gesellschaft für Anlagen und
Reaktorsicherheit (GRS gGmbH), 38122 Braunschweig, Germany
Dieter Schild
Institute for Nuclear Disposal, Karlsruhe Institute of Technology
(KIT), 76344 Eggenstein-Leopoldshafen, Germany
Related authors
No articles found.
Natalia Mayordomo, Diana M. Rodríguez, Vinzenz Brendler, André Rossberg, Andreas C. Scheinost, Dieter Schild, Irene Cardaio, Arkadz Bureika, Caroline Börner, and Katharina Müller
Saf. Nucl. Waste Disposal, 2, 155–156, https://doi.org/10.5194/sand-2-155-2023, https://doi.org/10.5194/sand-2-155-2023, 2023
Short summary
Short summary
In the last few years, we have studied the immobilization of the long-lived fission product technetium-99 (99Tc) by various Fe(II) minerals. Those minerals enable the reduction of Tc(VII) to Tc(IV), which is crucial to decrease the migration of technetium in the environment. In the future, we want to analyze Tc immobilization strategies under more complex systems that could, in a more realistic way, improve environmental conditions.
Nicolas Finck, Nikoleta Morelová, Michel L. Schlegel, Dieter Schild, Solenn Reguer, Kathy Dardenne, and Horst Geckeis
Saf. Nucl. Waste Disposal, 2, 39–40, https://doi.org/10.5194/sand-2-39-2023, https://doi.org/10.5194/sand-2-39-2023, 2023
Short summary
Short summary
Stainless steel was exposed to highly saline brines under anoxic and elevated temperature conditions. Samples were analyzed by various techniques in order to identify the nature of the secondary phases present in the corrosion layer forming at the steel–brine interface. Outcomes suggest that the corrosion layer has duplex structure, with an inner layer mostly of chromium (hydr)oxides and an outer layer made of iron- and nickel-based spinel compounds with admixed nickel (hydr)oxides.
Tobias König, Ron Dagan, Kathy Dardenne, Michel Herm, Volker Metz, Tim Pruessmann, Jörg Rothe, Dieter Schild, Arndt Walschburger, and Horst Geckeis
Saf. Nucl. Waste Disposal, 1, 5–6, https://doi.org/10.5194/sand-1-5-2021, https://doi.org/10.5194/sand-1-5-2021, 2021
Nikoleta Morelová, Kathy Dardenne, Nicolas Finck, Frank Heberling, Volker Metz, Dieter Schild, Horst Geckeis, and Nikitas Diomidis
Saf. Nucl. Waste Disposal, 1, 103–104, https://doi.org/10.5194/sand-1-103-2021, https://doi.org/10.5194/sand-1-103-2021, 2021
Short summary
The corrosion process of spherical graphite cast steel GGG40 bentonite saturated with Opalinus Clay pore water was investigated in a specially designed electrochemical cell, which allows the corrosion rate to be monitored in medium-term experiments. The morphology and chemistry of the interface was inspected by means of electron microscopy and surface chemical spectroscopy. This study supports the evaluation of this material's chemical and physical integrity for repository containers.
The corrosion process of spherical graphite cast steel GGG40 bentonite saturated with Opalinus...